Number 383
25
Parameter | Method | Method details | Depth | Value | Text | Error | ||
---|---|---|---|---|---|---|---|---|
From | To | |||||||
SiO2 [%] | XRF | 205.60 | 23.83 | |||||
TiO2 [%] | XRF | 205.60 | 0.3 | |||||
Al2O3 [%] | XRF | 205.60 | 6.85 | |||||
Fe2O3total [%] | XRF | 205.60 | 2.77 | |||||
MnO [%] | XRF | 205.60 | 0.03 | |||||
MgO [%] | XRF | 205.60 | 8.85 | |||||
CaO [%] | XRF | 205.60 | 21.58 | |||||
Na2O [%] | XRF | 205.60 | 0.26 | |||||
K2O [%] | XRF | 205.60 | 2.12 | |||||
P2O5 [%] | XRF | 205.60 | 0.04 | |||||
S [%] | XRF | 205.60 | 0.3 | |||||
CO2 [%] | XRF | 205.60 | 32.02 | |||||
Cl [%] | XRF | 205.60 | 0.1 | |||||
Insoluble residue [%] | Insoluble residue by gravimetric method | 205.60 | 28.74 | |||||
FeO [%] | Titration method | 205.60 | 0.18 | |||||
Dry density [kg/m3] | density and porosity analysis | 205.60 | 2357 | |||||
Wet density [kg/m3] | density and porosity analysis | 205.60 | 2517 | |||||
Grain density [kg/m3] | density and porosity analysis | 205.60 | 2805 | |||||
Porosity [%] | density and porosity analysis | 205.60 | 15.99 | |||||
P-wave velocity [m/sec in dry sample] | P- and S-wave velocity | 205.60 | 2975 | |||||
P-wave velocity [m/sec in wet sample] | P- and S-wave velocity | 205.60 | 2785 |