Analysis (density and porosity analysis) from sample 101993
Method | density and porosity analysis |
Person/Institution | Shogenov |
Sample number | 101993 |
Remarks | Density and porosity were determined using the water saturation method. For density measurements samples were dried at a temperature 100110 °C and the weight of dry samples (Pd) was determined. Then the samples were saturated with water for 7 days and after that weighed in air (Pw) and water (Pww). From the obtained measurements the following parameters were calculated: dry density = Pd/V = Pd/(Pw Pww), where V represents sample volume; wet density= Pw/(Pw Pww); grain density= Pd/(Pd Pww); effective porosity = (Pw Pd)/(Pw Pww). Research Institute of Earths Crust of St, Petersburg University (Russia) |
Reference | Shogenova et al., 2005a |
Dataset | Geochemistry and petrophysics of the Mehikoorma core |
Locality | Mehikoorma 421 borehole |
Depth | 164.1 |
Stratigraphy | Narva Stage |
Lithostratigraphy | Leivu Formation |
Institution | Department of Geology, TalTech |
Date added | 2013-10-28 |
Date changed | 2014-01-10 |