Analüüs (märgkeemia) proovist F225-1105
Üldinfo
Metoodika | märgkeemia |
Proovi nr |
F225-1105
|
Viide | Koppelmaa et al., 1979 |
Lokaliteet |
Sonda F-225 puurauk
|
Sügavus | 298.3 |
Süg. kuni | 298.3 |
Stratigraafia |
Proterosoikum
|
Asutus | Eesti Geoloogiateenistus |
Kirje lisatud | 2022-11-30 |
Tulemused
Parameeter | Väärtus | Tekst | Viga |
---|---|---|---|
SiO2 [%] | 65.4 | 0.01 | |
TiO2 [%] | 0.83 | 0.01 | |
Al2O3 [%] | 14.9 | 0.01 | |
Fe2O3 [%] | 0.6 | 0.01 | |
FeO [%] | 3.02 | 0.01 | |
MnO [%] | 0.01 | 0.01 | |
MgO [%] | 1.04 | 0.01 | |
CaO [%] | 2.02 | 0.01 | |
Na2O [%] | 2.86 | 0.01 | |
K2O [%] | 8.52 | 0.01 | |
P2O5 [%] | 0.07 | 0.01 | |
S [%] | 0.1 | 0.01 | |
LOI [%] | 0.58 | 0.01 | |
SUM [%] | 99.95 | 0.01 | |
Fe2O3T [%] | 3.96 | 0.01 |